Science and Technology of Welding and Joining, Vol. 26, No. 4, out now
With papers looking at on microstructure and properties, shipbuilding steels, and Self-piercing riveting.
This issue contains the following articles, which are available to members via My IOM3.
Impact of Nb on microstructure and properties of oscillating laser-CMT hybrid welding joints of A7204P-T4 aluminium alloy sheets
Shikai Wu, Zhongxiu Li, Enyu Qi, Xujian Cui, Song Zhang & Xiaohui Han
Pages: 273-278
DOI: 10.1080/13621718.2021.1894764
Dynamic estimation of joint penetration by deep learning from weld pool image
Yongchao Cheng, Shujun Chen, Jun Xiao & YuMing Zhang
Pages: 279-285
DOI: 10.1080/13621718.2021.1896141
Formation of the periodic material flow behaviour in friction stir welding
Hao Su, Tao Wang & Chuansong Wu
Pages: 286-293
DOI: 10.1080/13621718.2021.1902605
Effect of TiC particles on ductility dip cracking susceptibility of Ni-base superalloy
Jingqing Chen, Pengju Zhang, Tao Mo & Yu Wu
Pages: 294-300
DOI: 10.1080/13621718.2021.1902609
Self-piercing riveting for single-strap butt joints in similar aluminium alloys
Chengyu Song, Baoying Xing, Xiaocong He & Shipeng Wang
Pages: 301-308
DOI: 10.1080/13621718.2021.1905944
Strengthening and toughening strategies of weld metal for in-situ nanoparticle reinforced tin bronze alloy
X. H. Chen, Y. F. Ma, Y. J. Cheng, Z. D. Wang, M. Yang, W. W. Jiang & Y. D. Cao
Pages: 309-315
DOI: 10.1080/13621718.2021.1907024
Influence of welding HAZ microstructure on low-temperature impact fracture behaviour in C–Mn shipbuilding steel
Zuopeng Zhao, Xuteng Hu, Weidong Wen & Bin Wang
Pages: 316-323
DOI: 10.1080/13621718.2021.1907689
Nanoscale chromium carbides induced abnormal hardness in dissimilar metal welds
F. C. Liu, T. W. Nelson, S. L. McCracken & P. Minson
Pages: 324-331
DOI: 10.1080/13621718.2021.1907690
High speed X-ray observation of digital controlled submerged arc welding phenomena
Yohei Abe, Takahiro Fujimoto, Mitsuyoshi Nakatani, Hisaya Komen,
Masaya Shigeta & Manabu Tanaka
Pages: 332-340
DOI: 10.1080/13621718.2021.1908746
Solidification cracking susceptibility associated with a teardrop-shaped weld pool
Sindo Kou
Pages: 341-347
DOI: 10.1080/13621718.2021.1910179